In view of the pollution of unpaved road dust in the current mines, this study demonstrated the excellent dust suppression performance of the dust suppressant by testing the dynamic viscosity, penetration depth and mechanical properties of the dust suppressant, and apply molecular dynamics simulations to reveal the interactions between substances. The results showed that the maximum dust suppression rate was 97.75 % with a dust suppressant formulation of 0.1 wt% SPI + 0.03 wt% Paas + NaOH. The addition of NaOH disrupts the hydrogen bonds between SPI molecules, which allows the SPN to better penetrate the soil particles and form effective bonding networks. The SPI molecules rapidly absorb onto the surface of soil particles through electrostatic interactions and hydrogen bonds. The crosslinking between SPI molecules connects multiple soil particles, forming larger agglomerates. The polar side chain groups in the SPN interact with soil particles through dipole-dipole interactions, further stabilizing the agglomerates and resulting in an enhanced dust suppression effect. Soil samples treated with SPN exhibited higher compressive strength values. This is primarily attributed to the stable network structure formed by the SPN dust suppressant within the soil. Additionally, the SPI molecules and sodium polyacrylate (Paas) molecules in SPN contain multiple active groups, which interact under the influence of NaOH, restricting the rotation and movement of molecular chains. From a microscopic perspective, the SPN dust suppressant further strengthens the interactions between soil particles through mechanisms such as liquid bridge forces, which contribute to the superior dust suppression effect at the macroscopic level.

期刊论文 2025-08-15 DOI: 10.1016/j.conbuildmat.2025.142163 ISSN: 0950-0618
  • 首页
  • 1
  • 末页
  • 跳转
当前展示1-1条  共1条,1页